My question is, is this actually 48u,
According to their chart :
80T/200 is 79u microns if I am reading it right.
If you are making rosin, you can make a small 2" x 2" 25u ss screen, fold it in half with rosin inside, then I fold over the top edge and then the sides to lock it all in. heat to 150-160f and slow press it out. Expect to loose 25% or so in wax but it will be clean for pens.
Last edited: