I ordered a prepress and bags for about 50usd from China. Paid about 24euro in import duty, wasn't exactly pleased but is what it is. I want a circular prepress to try but if they don't have in EU I will buy off brand
Dabpress 90micron ones, I'm having repress and still the corners and sides are holding oil.
10g at 75c 0.98
Repress at 85c 0.36
And still seeing more but had a blow out after the 85 repress
I'm using the rectangular pre press which I'm still not convinced is the right size for the recommended bags as there's a lot of gap between the pressed material and the seam of the bag since the bags are wider than the mould
I have the 10ton press with the recommended pump with a gauge that goes way past where I think I need to be, do you know the max psi I should go for with these plates if talking a 2x3.5"puck? Struggling with the maths :doh:
Does anyone freeze material to help with yield? I read about it but when applying heat from the plates I don't see how it helps, getting OK results at 90c but it's quite a dark return, 70/80 is much better but significantly less yield