I also use an ultrasonic. I use small 2" X 3" zipper bags of 1/2 hot water 1/2 Dawn Platinum mixed, or zipper sandwich bags of the same mix in hot water in a small ultrasonic like for glasses for 2 to 3 five minute cycles. No replacement o-rings needed in a year or so.
I turned a bottle of iso over on my countertop and did not realize until the next day. I had a cooking thermometer turned face down next to it and the clear lens turned white and opaque. After months of procrastinating I was about to get an RMA to have it fixed, went to get it to have in hand...
https://www.mcmaster.com/screens/stainless-steel-wire-cloth-discs/ is the link to the round screen page on MacMaster-Carr's website. As I stated 1/2" part # 9317T124
1st column 4 down
If you have time look at all that they have.
notams,
Thanks for the welcome and for the tip for another place for screens. I just ordered some 1/2" today for my Bowle 60 mesh.
I don't like to run out of anything that I can get to keep things chugging along.
Thanks SS. I have used Delta 3D a bunch. I did not think of them and wasn't sure of weave and stiffness. I'm just waiting to see what they are going to come up for my Bowle and TM.
I'm a long time lurker and learner here and I want to say thanks to all that have posted and therefore taught me.
The reason I am posting now is that when receiving my new OAB the first thing noticed was how fast the screen clogged. Took it out and it is a much finer weave than the one that came...